Photopolymer

  • siladan010
  • Jun 11
  • 1 min read
ree


I started working on this polymer plate last week


Run few test prints to set the exposure, I have the results documented s somewhere in my phone


the best results on the exposure unit at CSMwhere


70 units of light (which are classed as seconds but took longer than 70 seconds so I called them units) for expire the aquatint screen


Second step was expose for 37 units the acetate film


Third stage was develop - just wash with water


Than ink the plate and print



This was the second run


I was playing with adding yellow and blue to the black ink to create a bit of mudy colour and texture in the greys


Compared with the inkjet the prints is a bit softer but that’s what I wanted


As for now I love the print



ree


ree

ree

 
 

Recent Posts

See All
To my peers

Two years of Thursdays afternoons of faces framed in zoom boxes layout. Two years of breakout rooms with some joyous, some tedious, some...

 
 

siladanCSM

©2023 by siladanCSM

 created with Wix.com

bottom of page